Basic principle: The cathode reaction is divided into two processes: 1. Water or hydrogen ions are first reduced to produce the intermediate product hydrogen atoms. This step is the key to determining the difficulty of the reaction. 2. The hydrogen atoms are then combined into hydrogen molecules, which is hydrogen gas.

For example, an electrolytic cell composed of two graphite electrodes usually requires a voltage greater than 2 V to produce hydrogen and oxygen, because graphite is not an ideal catalyst, while an electrolytic cell composed of two stainless steel electrodes requires a voltage of about 1.6-1.8V to produce hydrogen and oxygen. Hydrogen and oxygen. Researching new catalysts to increase energy conversion efficiency is a focus of great attention in the energy field.
In an acidic environment, platinum is a catalyst for the hydrogen evolution reaction. It has almost no overpotential and a very small Tafel slope (the additional voltage required to increase the current by 10 times). It is an almost ideal catalyst. However, due to the scarcity of platinum precious metal resources , scientists are looking for some cheap catalysts (transition metal sulfides, carbides and phosphides).
For example, nickel-based alloys exhibit excellent catalytic activity and stability for hydrogen evolution reaction, and nickel-iron-based composite materials and some perovskite materials exhibit excellent catalytic activity for oxygen evolution reaction.
The corresponding electrons flow from the positive electrode to the negative electrode through the external circuit. For the commercial use of hydrogen fuel cells, one of the biggest challenges is cost control. The current cost of fuel cell vehicles is about five times that of ordinary cars. Its core component is called the proton exchange membrane. It can separate electrons in hydrogen into protons, and then exchange them from the positive electrode to the negative electrode to react with oxygen to produce water and heat. Correspondingly, the core of the proton exchange membrane is the catalyst platinum. Platinum is a precious metal, which is usually platinum, the material of wedding rings. In order to promote large-scale commercialization, on the one hand, the amount of catalyst must be reduced, and on the other hand, low-cost alternative materials must be sought.

In a platinum-based hydrogen fuel cell, hydrogen and oxygen are combined to generate electricity, with water and heat being the only by-products. Hydrogen and oxygen molecules react and combine through a proton exchange membrane (PEM) coated with a platinum catalyst.
Fuel cells share many of the same characteristics as batteries-quiet operation, no moving parts, and an electrochemical reaction that produces electricity. However, unlike batteries, fuel cells do not require charging and can operate indefinitely when fuel is available. A fuel cell can use a battery as a system component to store the electrical energy it generates.